Отрывок: b – The transmission spectra of Au nanoparticles synthesized on a c-Al2O3 substrate and the dependence of the spectral position ωp of the plasmon peak on the thickness d of the initial film (an insert). c - The photo of the Au nanoparticles step structure. The AFM-images of the silver nanoparticles synthesized on a sapphire substrate at the thicknesses d 1 nm (a) and 10 nm (b) of the initial Ag film are presented in fi...
Полная запись метаданных
Поле DC Значение Язык
dc.contributor.authorLotin, A.A.-
dc.contributor.authorNovodvorsky, O.A.-
dc.contributor.authorParshina, L.S.-
dc.contributor.authorKhramova, O.D.-
dc.contributor.authorMikhalevsky, V.A.-
dc.contributor.authorCherebilo, E.A.-
dc.date.accessioned2017-05-10 11:10:45-
dc.date.available2017-05-10 11:10:45-
dc.date.issued2017-
dc.identifierDspace\SGAU\20170505\63628ru
dc.identifier.citationLotin A.A. PLD creation of Au and Ag plasmonic nanoparticles / A.A. Lotin, O.A. Novodvorsky, L.S. Parshina, O.D. Khramova, V.A. Mikhalevsky, E.A. Cherebilo // Сборник трудов III международной конференции и молодежной школы «Информационные технологии и нанотехнологии» (ИТНТ-2017) - Самара: Новая техника, 2017. - С. 142-144.ru
dc.identifier.urihttp://repo.ssau.ru/handle/Informacionnye-tehnologii-i-nanotehnologii/PLD-creation-of-Au-and-Ag-plasmonic-nanoparticles-63628-
dc.description.abstractThe gold and silver plasmonic nanoparticles have been synthesized on the c-sapphire and silica substrates by the pulsed laser deposition method. It has been demonstrated that the variation of the thickness of as-grown gold and silver films permits producing the plasmon nanoparticles with different size and density. It provides the retuning of the frequency of surface plasmon resonance in wide spectral region.ru
dc.language.isoenru
dc.publisherНовая техникаru
dc.subjectplasmonic nanoparticlesru
dc.subjectsurface plasmon resonanceru
dc.subjectpulsed laser depositionru
dc.titlePLD creation of Au and Ag plasmonic nanoparticlesru
dc.typeArticleru
dc.textpartb – The transmission spectra of Au nanoparticles synthesized on a c-Al2O3 substrate and the dependence of the spectral position ωp of the plasmon peak on the thickness d of the initial film (an insert). c - The photo of the Au nanoparticles step structure. The AFM-images of the silver nanoparticles synthesized on a sapphire substrate at the thicknesses d 1 nm (a) and 10 nm (b) of the initial Ag film are presented in fi...-
Располагается в коллекциях: Информационные технологии и нанотехнологии

Файлы этого ресурса:
Файл Описание Размер Формат  
paper 32_142-144.pdfОсновная статья717.79 kBAdobe PDFПросмотреть/Открыть



Все ресурсы в архиве электронных ресурсов защищены авторским правом, все права сохранены.